Inorganic Ventures - We flex to your specs
Guide to Reliable Measurements  
 Home   Ordering   Tech Center  Inorganic Ventures and inorganic CRM's  Quotations  Inorganic Ventures and inorganic CRM's
Sign In | Register  Find out more on this analytical standards or certified reference material from IV Labs! Search   
 Guides & Articles   Periodic Table   Expert Advice    Links   Technical Support 
You are Here:  Tech Center > Guides and Articles > Part-Per-Billion Stability Study
  Technical Guides
 
ICP Operations
Reliable Measurements
Sample Introduction for ICP-MS and ICP-OES
Elemental Analysis of Zeolites
Silver Stability Facts
Pure Chlorite Developed by IV
Mercury Stability Facts
Part-Per-Billion Stability Study
Understanding Error Budgets
 
  Consumer Guides
 
Flexible Expiration Dates?
Investigate Credentials Before You Buy
What Makes a Site Secure?
Hazardous Shipping Guide
Certificate of Analysis Components
Expiration Facts You Should Know
Regulating Hazardous Materials
Credit Card Advantage
Shelf Life vs. Expiration Date
 
  Quality Management
 
NIST Traceability
ISO Simplified
Transition From QS-9000 to ISO/TS 16949:2000
Lean Operations to Trim Expenses
Impressions of Southeast Asia's Quality System
 
  Editorials and More
 
New Evaporation Device Shows Promise
Site More Friendly to Users
Industry After September 11th
Ion Chromatography SRMs in Danger
 
Part-Per-Billion Stability Study
Experimentation at the ppb Concentration Level in LDPE Bottles

By Paul Gaines, Ph.D. and Janis Tartalio  •  Edited by Brian Brolin

The purpose of this study was to determine the stability of elements at the ppb level in low density polyethylene (LDPE) bottles. The stability of metals at the ppb level in this container material was of consequential concern. In work reported previously, it was found that LDPE is the cleanest container material (see The Purity and Cleaning of Plastics for details) for trace metals solutions.


Experimental Design

  1. A blend of 65 elements from Inorganic Ventures / IV Labs' CMS-SET was prepared at the 0, 2, 10, and 100 ppb concentration level in 1 % (v/v) HNO3 at the start of the study.


  2. The set consists of the following;
    • CMS-1 - 10 µg/mL Ce, Dy, Er, Eu, Gd, Ho, La, Lu, Nd, Pr, Sm, Sc, Tb, Th, Tm, U, Yb, Y in 3.5 % HNO3
    • CMS-2 - 10 µg/mL Au, Ir, Pd, Pt, Re, Rh, Ru, and Te in 3.5 % HCl
    • CMS-3 - 10 µg/mL Ge, Hf, Mo, Nb, Ta, Sn, Ti, W, and Zr in 3.5 % HNO3 tr. HF
    • CMS-4 - 10 µg/mL Sb, As, Ba, Be, Bi, B, Cd, Ga, In, Pb, Se, Tl, and V in 3.5 % HNO3
    • CMS-5 - 10 µg/mL Ag, Al, Ca, Cs, Cr+3, Co, Cu, Fe, Li, Mg, Mn, Ni, K, Rb, Na, Sr, and Zn in 3.5 % HNO3

  3. Only LDPE bottles (500 mL) were used.


  4. The LDPE bottles were acid leached with 1% nitric acid for 59 hours at 60 °C. New blends prepared in the same way were compared to the original preparation at 1, 3, 25, 75, 137, 300, and 375 days.


  5. The New blends were compared to the original blend using ICP-MS and the relative % loss was calculated.


  6. The ICP-MS used is in a clean room limiting environmental contamination (opened 1 % nitric acid solutions in similar LDPE bottles placed around the auto-sampler yielded no detectable environmental contamination at times of ~ 100 hours).


  7. Measurements of each blend were made in the same LDPE bottle i.e. the blend was not exposed to any other container during the study.

Results

  1. Hg was not stable long enough to measure (minutes).


  2. Au was the next most unstable element, showing instability at the 2, 20, and 100 ppb levels at 3 days.


  3. Ag showed instability only at the 10 and 100 ppb levels at 137 days.


  4. Pd showed instability only at the 2 and 10 ppb levels at 3 days.


  5. Pt and Ta showed instability only at the 2 and 10 ppb levels at 137 days.


  6. Ir showed instability only at the 2 ppb level at 300 days.


  7. Mo, Sn, and Hf showed instability only at the 2 ppb level at 375 days.


  8. All other elements showed no instability at 2-100 ppb for 375 days, including:
    Ce, Dy, Er, Eu, Gd, Ho, La, Lu, Nd, Pr, Sm, Sc, Tb, Th, Tm, U, Yb, Y, Re, Rh, Ru, Te, Ge, Nb, Ti, W, Zr, Sb, As, Ba, Be, Bi, B, Cd, Ga, In, Pb, Se, Tl, V, Al, Ca, Cs, Cr+3, Co, Cu, Fe, Li, Mg, Mn, Ni, K, Rb, Na, Sr, and Zn.

Graphed data for each element that showed instability is available in our Reliable Measurements guide.


Observations

  • The 1 % nitric acid solutions of the alkali, alkaline, and rare earth elements do not show any instability at the 2-100 ppb level in LDPE.
  • The majority of elements studied were found to be stable for 1 year at the 2-100 ppb level.
  • Silver (Ag) is the only unstable element found that is stable at the 2 ppb level. Ag's instability is most likely linked to its chloride chemistry (photo-reduction, precipitation).
  • Gold (Au) and Mercury (Hg), which are similar in stability, are the most unstable elements and are the only elements unstable at all of the concentration levels studied. They are also reported to stabilize one another.
  • Platinum (Pt), Tantalum (Ta), Molybdenum (Mo), Tin (Sn), Hafnium (Hf), and Iridium (Ir) were originally present as a fluoride or chloride complex.

More Information

If you have questions about this study, e-mail our technical staff at ivtech@ivstandards.com or call us at 1-800-569-6799 and we'll be happy to discuss our data further. 


An Inorganic Ventures Publication - August 2001

 Privacy Policy  |  Site Map   
  800-569-6799   •   732-901-1900
© 2008 Inorganic Ventures, Inc.. All rights reserved.