Overcoming Gold Stability Issues

Peter had Au stability problems when diluting one of our multielement standards into calibration solutions with an HNO3 matrix. Most of the elements showed good calibration curves with ICP-MS, but Au often had too low intensities. He also found that after measuring his calibration solutions different times, the Au concentration increased. Peter wanted to know how he could overcome these Au stability problems.

Dear Peter,

Your question is a very good one. The problem is with the stability of Au in nitric acid media. We have found that there are only two elements that are not compatible with a 1% nitric acid matrix in a PE container at ppb concentration levels -- Au and Hg. Both elements chemi-adsorb on the container walls and are not stable for a 24 hour time period (refer to Part 7 of our Trace Analysis Guide, Stability of Elements at ppb Concentration Levels).

As the concentration of the Au increases, the relative stability improves to the point that a 100 ppb solution can be used the next day but will not be stable for 72 hours. The stability continues to improve as the Au concentration increases to the point that a 1000 ppm Au solution in nitric acid will be chemically stable for more than 12 months. It appears that the surface of a PE container can take up to ~ 100 micrograms of Au or Hg before adsorption ceases (this is not a number that we have validated, but rather have deduced from stability studies - in fact the loss through chemi-adsorption is an assumption on my part at this time).

The only solution to this problem that we have found thus far is to use an HCl matrix for both Au and Hg. The use of 1% v/v HCl solution rather than nitric acid should eliminate this problem. We are currently using a 10% v/v HCl matrix for ppb Au and Hg but we believe this is far more than needed. We have not yet initiated studies at lower HCl levels.

Please feel free to contact me with any further discussion on this or any related topic.

Serving you in chemistry,
Paul R. Gaines Paul R. Gaines, Ph.D.
CEO of Inorganic Ventures & Fellow Chemist

DISCLAIMER: Advice offered by the chemists at Inorganic Ventures is intended for the individual posing the question. Feel free to contact us to verify whether these suggestions apply to your unique circumstances.

Further Reading

Have a question?

Share your analytical chemistry problem with our experienced team of scientists, including well-known spectroscopist Dr. Paul Gaines. Note that while we make an effort to respond to every question, customers of Inorganic Ventures are always given priority.

Follow us on TwitterBecome a fan on FacebookSubscribe to our feed

Fully ISO Accredited

Get the IV Line eNewsletter!

Save up to 50% off at Inorganic Ventures

Request an Inorganic Ventures catalog
Inorganic Ventures spectrum